Abrasive wear behaviour of conventional and nanocomposite HVOF-sprayed WC–Co coatings DA Stewart, PH Shipway, DG McCartney Wear 225, 789-798, 1999 | 526 | 1999 |
Corrosion resistance of zinc–magnesium coated steel NC Hosking, MA Ström, PH Shipway, CD Rudd Corrosion science 49 (9), 3669-3695, 2007 | 484 | 2007 |
Internal combustion engine cold-start efficiency: A review of the problem, causes and potential solutions A Roberts, R Brooks, P Shipway Energy conversion and management 82, 327-350, 2014 | 434 | 2014 |
Microstructural evolution in thermally sprayed WC–Co coatings: comparison between nanocomposite and conventional starting powders DA Stewart, PH Shipway, DG McCartney Acta Materialia 48 (7), 1593-1604, 2000 | 430 | 2000 |
Bonding mechanisms in cold spraying: the contributions of metallurgical and mechanical components T Hussain, DG McCartney, PH Shipway, D Zhang Journal of Thermal Spray Technology 18, 364-379, 2009 | 417 | 2009 |
Sliding wear behaviour of conventional and nanostructured HVOF sprayed WC–Co coatings PH Shipway, DG McCartney, T Sudaprasert Wear 259 (7-12), 820-827, 2005 | 312 | 2005 |
Contact-evolution based prediction of fretting fatigue life: effect of slip amplitude JJ Madge, SB Leen, IR McColl, PH Shipway Wear 262 (9-10), 1159-1170, 2007 | 251 | 2007 |
The effect of temperature on wear and friction of a high strength steel in fretting SR Pearson, PH Shipway, JO Abere, RAA Hewitt Wear 303 (1-2), 622-631, 2013 | 230 | 2013 |
The role of particle properties in the erosion of brittle materials PH Shipway, IM Hutchings Wear 193 (1), 105-113, 1996 | 225 | 1996 |
Influence of heat treatment on the abrasive wear behaviour of HVOF sprayed WC–Co coatings DA Stewart, PH Shipway, DG McCartney Surface and Coatings Technology 105 (1-2), 13-24, 1998 | 203 | 1998 |
Microstructure and abrasive wear behaviour of shielded metal arc welding hardfacings used in the sugarcane industry VE Buchanan, PH Shipway, DG McCartney Wear 263 (1-6), 99-110, 2007 | 199 | 2007 |
The effect of particle hardness and shape when abrasive water jet milling titanium alloy Ti6Al4V G Fowler, IR Pashby, PH Shipway Wear 266 (7-8), 613-620, 2009 | 198 | 2009 |
Production of titanium deposits by cold-gas dynamic spray: numerical modeling and experimental characterization T Marrocco, DG McCartney, PH Shipway, AJ Sturgeon Journal of Thermal Spray Technology 15, 263-272, 2006 | 181 | 2006 |
Fracture of brittle spheres under compression and impact loading. I. Elastic stress distributions PH Shipway, IM Hutchings Philosophical Magazine A 67 (6), 1389-1404, 1993 | 180 | 1993 |
Microscale abrasive wear of polymeric materials PH Shipway, NK Ngao Wear 255 (1-6), 742-750, 2003 | 174 | 2003 |
Cold gas dynamic spraying of aluminum: the role of substrate characteristics in deposit formation D Zhang, PH Shipway, DG McCartney Journal of thermal spray technology 14, 109-116, 2005 | 172 | 2005 |
Mechanical stabilisation of bainite PH Shipway, H Bhadeshia Materials science and technology 11 (11), 1116-1128, 1995 | 169 | 1995 |
Three-body abrasive wear of fine pearlite, nanostructured bainite and martensite SD Bakshi, PH Shipway, H Bhadeshia Wear 308 (1-2), 46-53, 2013 | 166 | 2013 |
Sliding wear behaviour of electrodeposited cobalt–tungsten and cobalt–tungsten–iron alloys H Capel, PH Shipway, SJ Harris Wear 255 (7-12), 917-923, 2003 | 162 | 2003 |
Friction and sliding wear behaviour of electrodeposited cobalt and cobalt–tungsten alloy coatings for replacement of electrodeposited chromium DP Weston, PH Shipway, SJ Harris, MK Cheng Wear 267 (5-8), 934-943, 2009 | 161 | 2009 |