Control of MgO· Al2O3 spinel inclusions in stainless steels JH Park, H Todoroki ISIJ international 50 (10), 1333-1346, 2010 | 423 | 2010 |
Effect of silica in slag on inclusion compositions in 304 stainless steel deoxidized with aluminum H Todoroki, K Mizuno ISIJ international 44 (8), 1350-1357, 2004 | 159 | 2004 |
Effects of Al and Ca in ferrosilicon alloys for deoxidation on inclusion composition in type 304 stainless steel K Mizuno, H Todoroki, M Noda, T Tohge Iron and Steelmaker(USA) 28 (8), 93-101, 2001 | 120 | 2001 |
Variation of inclusion composition in 304 stainless steel deoxidized with aluminum H Todoroki, K Mizuno Iron & steelmaker 30 (3), 60-67, 2003 | 79 | 2003 |
Effect of crystallization behavior of mold flux on slab surface quality of a Ti-bearing Fe–Cr–Ni super alloy cast by means of continuous casting process H Todoroki, T Ishii, K Mizuno, A Hongo Materials Science and Engineering: A 413, 121-128, 2005 | 66 | 2005 |
Application of extreme value analysis for two-and three-dimensional determinations of the largest inclusion in metal samples Y Kanbe, A Karasev, H Todoroki, PG Jönsson ISIJ international 51 (4), 593-602, 2011 | 62 | 2011 |
Effect of rare earth metal on inclusion composition in molten stainless steel A Katsumata, H Todoroki Iron & steelmaker 29 (7), 51-57, 2002 | 51 | 2002 |
Rapid measurement scheme for texture in cubic metallic materials using time-of-flight neutron diffraction at iMATERIA Y Onuki, A Hoshikawa, S Sato, PG Xu, T Ishigaki, Y Saito, H Todoroki, ... Journal of Applied Crystallography 49 (5), 1579-1584, 2016 | 49 | 2016 |
Recent innovation and prospect in production technology of specialty steels with high cleanliness H Todoroki, S Inada Bull. Iron Steel Inst. Jpn 8 (8), 575-580, 2003 | 40 | 2003 |
Microwave carbo-thermal reduction for recycling of Cr from Cr-containing steel making wastes N Yoshikawa, K Mashiko, Y Sasaki, S Taniguchi, H Todoroki ISIJ international 48 (5), 690-695, 2008 | 38 | 2008 |
Analysis of largest sulfide inclusions in low carbon steel by using statistics of extreme values Y Kanbe, A Karasev, H Todoroki, PG Jönsson steel research international 82 (4), 313-322, 2011 | 37 | 2011 |
Estimation of microwave penetration distance and complex permittivity of graphite by measurement of permittivity and direct current conductivity of graphite powder mixtures N Yoshikawa, K Kawahira, Y Saito, H Todoroki, S Taniguchi Journal of Applied Physics 117 (8), 2015 | 34 | 2015 |
Melting behavior of siliceous nickel ore in a rotary kiln to produce ferronickel alloys Y Kobayashi, H Todoroki, H Tsuji ISIJ international 51 (1), 35-40, 2011 | 32 | 2011 |
Formation mechanism of spinel type inclusion in 304 stainless steel deoxidized with ferrosilicon alloys H Todoroki, K Mizuno, M Noda, T Tohge Steelmaking Conference Proceedings 84, 331-342, 2001 | 32 | 2001 |
Prevention of longitudinal cracks in a continuously cast slab of Fe–Cr–Ni superalloy containing Al and Ti Y Kanbe, T Ishii, H Todoroki, K Mizuno International Journal of Cast Metals Research 22 (1-4), 143-146, 2009 | 29 | 2009 |
Initial solidification ofiron, nickel and steel droplets H Todoroki, R Lertarmon, AW Cramb, T Suzuki Iron and Steelmaker 26, 57, 1999 | 24 | 1999 |
Effect of compositions of non-metallic inclusions on CC nozzle clogging of a Fe-Cr-Ni-Mo system stainless steel H Todoroki, F Kirihara, Y Kanbe, Y Miyazaki TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN 100 (4 …, 2014 | 23 | 2014 |
Dehydration behavior of goethite blended with graphite by microwave heating Y Saito, K Kawahira, N Yoshikawa, H Todoroki, S Taniguchi ISIJ international 51 (6), 878-883, 2011 | 21 | 2011 |
Solubility of nitrogen in Fe–Cr–Ni–Mo stainless steel under a 1 atm N2 gas atmosphere Y Kobayashi, H Todoroki, N Shiga, T Ishii ISIJ international 52 (9), 1601-1606, 2012 | 20 | 2012 |